20Khz Ultrasonic Spot Metal Welder for Braided Wire with Special
Steel Welding Horn
Description:
Ultrasonic metal welding is a special welding method that uses
ultrasonic vibration (frequency over 18 kHz) to connect the same or
different metals, semiconductors, plastics, and cermets.
The ultrasonic metal welding process is a process between cold
press welding and friction welding that utilizes high density
energy generated by high frequency mechanical vibration. The
mechanical vibration of the welding head of the ultrasonic metal
welding is parallel to the surface of the workpiece. During
welding, the static pressure acts perpendicularly on the welding
surface through the welding head, and at the same time superimposes
the shearing force of the high-frequency vibration. When the
shearing force exceeds the elastic limit of the material, the part
of the contact surface of the workpiece begins to slip. This
shearing force The direction is constantly changed at a frequency
of tens of thousands of times per second during the welding
process. Breaking and removing dirt on the surface of the
workpiece, the surface of the pure metal begins to contact in
multiple points. As the high-frequency vibration continues, the
contact area of the pure metal expands until it expands into the
entire weld zone, and at the same time, atoms are formed on the
contact surface. Diffusion, metal recrystallization produces fine
grain structure and exhibits cold metal deformation
characteristics.
Specifications:
Item No | QR-D2020A | QR-D2030A | QR-D2050A |
Power | 2000W | 3000W | 5000W |
Air Pressure | 0.05-0.9MPa | 0.05-0.9MPa | 0.05-0.9MPa |
Frequency | 20KHZ | 20KHZ | 20KHZ |
Voltage | 220V | 220V | 380V |
Weight of horn | 55KG | 60KG | 88KG |
Dimension of Horn | 550*280*380mm | 550*280*430mm | 550*380*660mm |
Generator Size | 540*380*150mm | 540*380*150mm | 540*380*150mm |
common problem:
The welding head will have a certain heat phenomenon during work,
which is caused by the mechanical loss of the material itself and
the heat conduction of the weldment. Whether the welding hair heat
is normal or not, when the load is not loaded (ie, does not touch
the workpiece), the ultrasonic wave is continuously emitted for
more than half an hour, and the temperature cannot exceed 50-70 °
C. If the heat is severe, it proves that the welding head is
damaged or the material is unqualified. replace.
When there is a howling when the welding head is working, the
following reasons should be analyzed:
1. Is the mounting screw loose?
2. Does the weld head have cracks?
3. Whether the welding head is in contact with objects that should
not be in contact.
Ultrasonic metal welding products:
1. Nickel-metal hydride battery nickel-metal hydride battery nickel
mesh and nickel sheet inter-melting
2. Lithium battery, polymer battery copper foil and nickel sheet
inter-melting, aluminum foil and aluminum sheet inter-melting
3. The wires are mutually melted and are entangled into one and
more fuses.
4. Wire and various electronic components, contacts, connectors and
mutual melting
5. Large-scale heat sinks, heat exchange fins, and honeycomb cores
of various household appliances and auto accessories
6. Large current contacts such as electromagnetic switches and
non-fuse switches, and mutual melting of dissimilar metal sheets
7. Metal tube sealing, cutting can be water, airtight
8. Solar heat absorbing plate, aluminum-plastic composite pipe, and
aluminum plate splicing
20Khz Ultrasonic Spot Metal Welder for Braided Wire with Special
Steel Welding Horn